  • curprev 14:3614:36, 18 June 2026 Eves talk contribs 2,805 bytes +465 No edit summary
  • curprev 14:3414:34, 18 June 2026 Eves talk contribs 2,340 bytes +2,340 Created page with "=Anton Paar Stage - BTS 500= Anton Paar heating stage (BTS 500 - Benchtop Heating Stage) is a non-ambient sample stage for X-ray powder diffraction that allows temperature-controlled experiments. The sample chamber is mounted on the goniometer instead of the standard (ambient) sample holder to heat the sample to a defined temperature while scanning it with X-rays. BTS 500 enables X-ray scans to be performed from ambient temperature to 500 °C. The sample can be heated..."