  • curprev 14:3114:31, 6 April 2011 Jml talk contribs 197 bytes +197 Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 461, 462 and 463, time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs. 30 mm spacers