  • curprev 12:4112:41, 4 April 2011 Jml talk contribs 196 bytes +196 Etching of nanostructures in Si using the ICP metal etcher: Sinano3.31 recipe, Run ID 452(abc), 453(bc) and 454 (c), time 60, 120 and 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 50 degs.