Specific Process Knowledge/Thin film deposition/Deposition of Platinum
Appearance
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
Platinum deposition
Platinum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (E-beam evaporator (Temescal) and E-beam evaporator (10-pockets)) | Sputter deposition (Lesker) | Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | |
|---|---|---|---|
| General description | E-beam deposition of Pt | Sputter deposition of Pt | Sputter deposition of Pt |
| Pre-clean
|
Ar ion etch (only in E-beam evaporator Temescal) | none | RF Ar clean |
| Layer thickness | 10Å - 600nm* | 10Å - 600nm* | 10Å - ? discuss with staff |
| Deposition rate | 0.5Å/s to 10Å/s | up to 3.74 Å/s | not known yet, probably similar to 'old' Lesker system |
| Batch size |
|
|
|
| Allowed materials |
Almost any that does not degas at your intended substrate temperature. See the cross-contamination sheet. |
|
|
| Comment | Pt tends to exhibit tensile stress, see section on stress in thin films. |
* If depositing a total of more than 600 nm, please write to metal@nanolab.dtu.dk well in advance to ensure that enough material is present.