Specific Process Knowledge/Polymer Processing/Plasma Cleaners
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
Plasma cleaner: 2 & 3
Plasma cleaner 2 : SurfacePrep(located in PolyFaLab) and Plasma cleaner 3 : PDMS (located in PDMS lab) are Diener Atto (PC control, 13.56 MHz RF) systems installed in 2026.
The Plasma Cleaner 2 : SurfacePrep can be used for the following processes:
- Fine cleaning/surface activation of polymer parts prior to bonding, coating, printing
- Photoresist stripping
- Descumming
- Surface cleaning
The user manual, and contact information for plasma cleaner : 2 can be found in LabManager - requires login
The Plasma Cleaner 3 : PDMS can be used for the following processes:
- Surface activation and micro-etching of cured PDMS surface
- PDMS to glass bonding
For further information about PDMS to glass bonding follow the link: PDMS Casting
The user manual, and contact information for plasma cleaner : 3 can be found in LabManager - requires login
Plasma cleaner Comparison Table
| Plasma Cleaner 2 : Surfaceprep | Plasma Cleaner 3: PDMS | |
| Purpose | Cleaning/Surface activation before bonding, coating and printing | Surface activation and micro-etching of cured PDMS |
| Method | Low-pressure RF plasma | Low-pressure RF plasma |
| Process gasses |
|
|
| Process power | 10-300 W (10-100%) | 10-300 W (10-100%) |
| Process pressure | 0.35 mbar | 0.35 mbar |
| Substrate batch |
|
|
| Substrate materials |
|
|