Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour. Result from Trine H. Christensen DTU Space
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 16:04, 17 February 2015 | 1,164 × 938 (31 KB) | Paphol (talk | contribs) | Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour. Result from Trine H. Christensen DTU Space |