AFM picture of Cr layer sputter deposited in Wordentec. Settings: 405W, 0.004mbar

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current09:14, 13 August 2008Thumbnail for version as of 09:14, 13 August 2008795 × 628 (97 KB)Kn (talk | contribs)AFM picture of Cr layer sputter deposited in Wordentec. Settings: 405W, 0.004mbar