Specific Process Knowledge/Etch/Etching of Chromium
Appearance
Feedback to this page: click here
Etching of Chromium
Etching of chromium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Chromium Etch Metods
| Cr wet etch 1 | Cr wet etch 2 | ICP metal | IBE (Ionfab300+) | |
|---|---|---|---|---|
| Generel description | Wet etch of Cr premixed (Chrome etch 18) | Wet etch of Cr that you need to mix your self | Dry plasma etch of Cr | Sputtering of Cr - pure physical etch |
| Etch rate range |
|
|
|
|
| Etch profile |
|
|
|
|
| Substrate size |
|
|
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |