KOH Etch
|
Wet PolySilicon etch
|
RIE (Reactive Ion Etch)
|
DRIE-Pegasus (Silicon Etch)
|
ASE (Advanced Silicon Etch)
|
ICP Metal Etch
|
IBE/IBSD Ionfab 300
|
| Generel description
|
- Anisotropic etch in the (100)-plan
- High selectivity to the other plans
- Anisotropic etch: vertical sidewalls independent of the crystal plans
|
- Isotropic etch in Silicon and Polysilicon
|
- Can etch isotropic and anisotropic depending on the process parameters
|
- State-of-the-art dry silicon etcher with atmospheric cassette loader
- Extremely high etch rate and advanced processing options
|
- As RIE but better for high aspect ratio etching and deep etches (higher etch rate)
- Good selectivity to photoresist
- The ASE is dedicated to polymer etch, which can affect the Si etch stability.
|
- This is dedicated to metal etch. So fare only Si etch of nanostructures has been explored on the system.
|
- Primarily for pure physical etch by sputtering with Ar-ions
|
| Possible masking materials
|
- Silicon Nitride
- Silicon Oxide
|
|
- Photoresist
- E-beam resist
- Silicon Oxide
- Silicon Nitride
- Aluminium
- Chromium (ONLY RIE2!)
- Other metals if they cover less than 5% of the wafer area (ONLY RIE2!)
|
- Photoresist and zep resist
- Silicon Oxide
- Silicon Nitride
- Aluminium oxide
|
- Photoresist
- Silicon Oxide
- Silicon Nitride
- Aluminium
|
- Photo-, DUV- and e-beamresist
- Silicon Oxide
- Silicon Nitride
- Aluminium
- Cr
- Ti
|
- Any material that is accepted in the machine
|
| Etch rate range
|
- Si(100) @80oC: 1.29+0.05 µm/min
- Si(100) @70oC: ~0.7 µm/min
- Si(100) @60oC: ~0.4 µm/min
|
- ~100-200 nm/min, highly dependent on doping level
|
- <40nm/min to >600nm/min depending on recipe parameters and mask design
|
- Up to 18-20 µm/min depending on recipe, mask design and aspect ratio.
|
- <130nm/min to >5.6 µm/min depending on recipe, mask design and aspect ratio.
|
- Process dependant. The nano etch is in the range 59-311 nm/min
|
- Process dependant. Has been tested in the range 17-31 nm/min
|
| Substrate size
|
- 25 wafers of 100mm in our 100mm bath
- 1-5 wafers of 100mm or 50mm in "Fumehood KOH"
- 25 wafers of 100mm or 150mm in our 6" bath
|
- #25 100 mm wafers in our 100mm bath
|
- As many small samples as can be fitted on the 100mm carrier.
- 1 100mm wafer (or smaller with carrier)
- 1 150mm wafer (only when the system is set up for 150mm)
|
- As many small samples as can be fitted on a 100mm wafer
- #1 50 mm wafer fitted on a 100mm wafer
- #1 100 mm wafer
- #1 150 mm wafers (only when the system is set up to 150mm)
|
- As many small samples as can be fitted on a 100mm wafer
- #1 50 mm wafer fitted on a 100mm wafer
- #1 100 mm wafer
- #1 150 mm wafers (only when the system is set up to 150mm)
|
- As many small samples as can be fitted on a 150mm wafer
- #5 50 mm wafer fitted on a 150mm wafer
- #1 100 mm wafer on a 150mm wafer
- #1 150 mm wafers (The system is normally set up to 150mm)
|
- As many samples as can be securely fitted on a up to 200mm wafer
- #1 50 mm wafer with special carrier
- #1 100 mm wafer with special carrier
- #1 150 mm wafers with special carrier
- #1 200 mm wafer
|
| Allowed materials
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Other materials (only in "Fumehood KOH")
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
- Other metals if they cover less than 5% of the wafer area (ONLY RIE2!)
- Quartz/fused silica
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- zep resist
- Aluminium oxide
- Quartz/fused silica
|
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
- Aluminium
- Quartz/fused silica
|
- Silicon
- Photoresist/e-beam resist
- PolySilicon
- Silicon oxide
- Silicon (oxy)nitride
- Aluminium
- Titanium
- Chromium
- Quartz/fused silica
|
- Silicon
- Silicon oxides
- Silicon (oxy)nitrides
- Metals from the +list
- Metals from the -list
- Alloys from the above list
- Stainless steel
- Glass
- III-V materials
- Resists
- Polymers
- Capton tape
|