Revision as of 22:02, 3 December 2007 by Jml (talk | contribs) (Sample info: Nanoimprintede cantilevers i topas monteret på en SU8 chip)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 943 pixels, file size: 71 KB, MIME type: image/jpeg)

Sample info: Nanoimprintede cantilevers i topas monteret på en SU8 chip

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current22:09, 3 December 2007Thumbnail for version as of 22:09, 3 December 20071,024 × 943 (71 KB)Jml (talk | contribs)A TOPAS cantilever mounted on a SU8 base chip
22:02, 3 December 2007Thumbnail for version as of 22:02, 3 December 20071,024 × 943 (71 KB)Jml (talk | contribs)Sample info: Nanoimprintede cantilevers i topas monteret på en SU8 chip