File:IBE-Si-CA-contour.jpg

From LabAdviser
Revision as of 09:59, 10 December 2012 by Khr (talk | contribs) (The angle in the corner of an etch structure showed a dependency on Beam and Acc. Voltage and Incident angle, with no interactions between any parameters. Values found on the plot should always be tested before use.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,890 × 945 pixels, file size: 725 KB, MIME type: image/jpeg)

The angle in the corner of an etch structure showed a dependency on Beam and Acc. Voltage and Incident angle, with no interactions between any parameters. Values found on the plot should always be tested before use.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current09:59, 10 December 2012Thumbnail for version as of 09:59, 10 December 20121,890 × 945 (725 KB)Khr (talk | contribs)The angle in the corner of an etch structure showed a dependency on Beam and Acc. Voltage and Incident angle, with no interactions between any parameters. Values found on the plot should always be tested before use.

Metadata