BCB Curing Oven
The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of metals in a nitrogen atmosphere.
During processing the furnace is rapidly heated by use of eight halogen lamps situated below the sample. The furnace is purged with a high or a low nitrogen flow. Samples are processed at atmospheric pressure or at vacuum.
The user manual, user APV, technical information and contact information can be found in LabManager:
Process information
There are no standard processes on the furnace.
| Equipment | BCB Curing Oven | |
|---|---|---|
| Purpose |
| |
| Process parameter range | Temperature |
|
| Nitrogen flows |
| |
| Pressure |
| |
| Substrates
(Remember to use the right carrier wafer) |
Batch size |
|
| Allowed materials |
| |