Revision as of 12:20, 12 January 2026 by Jehem (talk | contribs) (Created page with "=Resist Strip= 400px|thumb|Resist strip bench in D-3 This resist strip is only for wafers without metal and SU-8. There are one Remover 1165 bath for stripping and one IPA bath for rinsing. '''Here are the main rules for resist strip use:''' *Place the wafers in a wafer holder and put them in the first bath for 10 min, this time is depending how much resist you have on the surface. *After the strip rinse your wafers in the IPA bath for 2-3...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Resist Strip

 
Resist strip bench in D-3

This resist strip is only for wafers without metal and SU-8.

There are one Remover 1165 bath for stripping and one IPA bath for rinsing.

Here are the main rules for resist strip use:

  • Place the wafers in a wafer holder and put them in the first bath for 10 min, this time is depending how much resist you have on the surface.
  • After the strip rinse your wafers in the IPA bath for 2-3 min.
  • Rinse your wafers for 4-5 min. in running water after stripping.


The user manual and contact information can be found in LabManager: Resist Strip - requires login