Revision as of 11:21, 12 January 2026 by Jehem (talk | contribs) (Created page with "==Inclined UV Lamp== 300x300px|right|thumb|Inclined UV lamp is placed in CX-1 The Inclined UV lamp is 1000 W Hg(Xe)lamp source designed for near UV, 350-450nm, mid UV, 260-320nm, and deep UV, 220-260nm exposures of resists and polymers. The exposure source can also be used to make an inclined exposure in air or in the media tank. The tool was purchased in February 2009 from Newport. The exposure lamp official name is Oriel Flood Exposure...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Inclined UV Lamp

 
Inclined UV lamp is placed in CX-1

The Inclined UV lamp is 1000 W Hg(Xe)lamp source designed for near UV, 350-450nm, mid UV, 260-320nm, and deep UV, 220-260nm exposures of resists and polymers. The exposure source can also be used to make an inclined exposure in air or in the media tank. The tool was purchased in February 2009 from Newport. The exposure lamp official name is Oriel Flood Exposure Source, unit 92540. All other parts of equipment: substrate and mask holder with media tank, exhaust box around the tool, timer controller, were designed and built at DTU Nanolab workshop.

The substrate and mask holder with a media tank was designed as part of Master Thesis of DTU Nanotech, Andres Kristensen group. The exhaust box was made for safety reasons and the timer/controller was built to control exposure time.

The technical specification and the general outline of the equipment can be found in LabManager.


The user manual(s), quality control procedure(s) and results and contact information can be found in LabManager - requires login

Equipment performance and process related parameters

Purpose

UV exposure

Performance Exposure mode
  • Flood exposure
  • Proximity exposure with mask possible for 4inch substrate
  • Inclined exposure
  • Rotating exposure
Exposure light/filters
  • Near UV(350-450nm)
  • Mid UV (260-320nm)
  • Deep UV(220-260nm)
Minimum structure size
Mask size

5x5inch optinal

Alignment modes

No alignment possible

Substrates Substrate size

Up to 8inch substrates, different shapes

Allowed materials

All cleanroom materials

Batch

1