Breakdown voltage results for the E1 8" Oxidation furnace

Dry oxidation

Date Oxidation recipe Oxide thickness Absolute break-down voltage Relative break-down voltage

= Absolute break-down voltage/oxide thickness

February 2022 DRY1050 117 nm
 
 
November 2023 DRY1100 510 nm
 
 
April 2025 DRY1050 115 nm
 
 

The break-down voltage measurements have been made with help from Kitty Steenberg and Rune Sixten Grass from DTU Health Tech.