Feedback to this page: click here Unless otherwise stated, the content of this page was created by the dry etch group at DTU Nanolab

XPS Knowledge View

The XPS Knowledge View shown here is from Avantage version 5.948.

 

  1. Click the knowledge view button in the toolbar to the left in Avantage as shown with a red square.
  2. A tab pops up in the window. Click on the periodic table as shown to select an element.