Barc etch with O2

Unless otherwise stated, all content in this section was done by Berit Herstrøm, DTU Nanolab, June 2020

Sample

  • 6" Si
  • 2 µm SiO2 from C1
  • 90 nm barc
  • 907 nm UVN 2030-0,5
  • Reticle: Pegreticle
  • Dose: 200 J/m2

Pegasus 4 settings

  • Recipe: Barc O2
  • With 30 mm spacers

SEM images after barc etching