Mask Specifications

Below you can find two examples on how to write the specification for 5" and 7" masks.

5" masks

All Layers:

5" chromium mask
fracture limits ((-50000, -50000),(50000, 50000))
Dark periphery
Chromium down

GDS-file: GLO006_v7.gds
Top cell: wafer

Layer (GDS number): 01
Mask Type: Digitised data= Dark, right reading
Text(max 30 characters): init-2019-Nitride-etch

Layer (GDS number): 02
Mask Type: Digitised data= Clear, Wrong reading
Text(max 30 characters): init-2019-KOH-backside

For 7" masks

All Layers:

7" chromium mask
fracture limits ((-70000, -70000),(70000, 70000))
Dark periphery
Chromium down

GDS-file: GLO006_v7.gds
Top cell: wafer

Layer (GDS number): 01
Mask Type: Digitised data= Dark, right reading
Text(max 30 characters): init-2019-Nitride-etch

Layer (GDS number): 02
Mask Type: Digitised data= Clear, Wrong reading
Text(max 30 characters): init-2019-KOH-backside