Etching Al2O3 can be done both chemically (wet) and by dry etching. Chemical etching can be done using BHF (60nm/min) or a developer (4nm/min). This will be selective to most materials not containing Al. We have done some test of Al2O3 in dry etching. It has been mostly tested in the III-V ICP and ICP Metal. Please see links below.