Etching of nanostructures in Si using DRIE-Pegasus: nano1.3 recipe, Run ID 1856 (a) and 1857 (a+b), time 60 secs (a) and 120 secs (b), SF6 38, C4F8 52, 4mtorr, 600/40 coil/platen, -10 degs.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current15:01, 30 March 2011Thumbnail for version as of 15:01, 30 March 20111,024 × 768 (104 KB)Jml (talk | contribs)Etching of nanostructures in Si using DRIE-Pegasus: nano1.3 recipe, Run ID 1856 (a) and 1857 (a+b), time 60 secs (a) and 120 secs (b), SF6 38, C4F8 52, 4mtorr, 600/40 coil/platen, -10 degs.

Metadata