Specific Process Knowledge/Wafer cleaning/Post CMP Cleaner
Appearance
Feedback to this page: click here
Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.
All links to Labmanager requires login.
Post CMP Cleaner)
The post CMP Cleaner is designed for removing slurry residues from polishing wafers. The Post CMP cleaner is the recommended cleaning tool after using the Polisher CMP.
The user manual, user APV, technical information and contact information can be found in LabManager:
| Equipment | Post CMP Cleaner | |
|---|---|---|
| Purpose |
Cleaning of |
|
| Process parameter range | ||
| Mechanical Cleaning |
| |
| Power |
| |
| Arm sweep |
| |
| Substrates | Sample size |
|
| Allowed materials |
| |