AZ MiR 701 is a positive UV photoresist.

Spin coating

 
Spin curves for AZ MiR 701 (29cps) using a 30s spin-off, and a 60s@90°C softbake (proximity bake for Gamma)


Post-exposure bake

During exposure, interaction between the incoming light and the light reflected by the substrate can cause a standing wave to form in the resist (especially true for single line/wavelength exposure). This leads to a wavy sidewall after development. The standing wave pattern can be removed by introducing a post-exposure bake before development, which allows the activated PAC to diffuse into un-activated regions, thus smoothing the sidewall. The recommended PEB for MiR is 60s at 110°C.

As the post-exposure bake is at an elevated temperature compared to the soft bake, it will cause the resist film to become 5-10% thinner (probably due to continued evaporation of solvent). A 1.5µm thick MiR resist film will be approximately 1.4µm after PEB.

Development

A 1.5-2µm MiR resist film is fully developed in 60s using TMAH (AZ 726). Thicker coatings will require longer development (1 min per 2µm).