Jump to content

Specific Process Knowledge/Characterization/Profiler

From LabAdviser

Dektak 8 stylus profiler

 
Dektak8: positioned in cleanroom 4 - glass cage no. 3

Dektak 8 stylus profiler is a product of Veeco Instruments. It is usable for profiling surfaces of samples with structures in the micrometer range. It can measure in a specific point found with help from high magnification video cameras or it can be programmed to measure several points defined with respect to some deskew points. It can also be used for stress measurements of thin films by measuring the wafer bow.

To get some product information and some tips and tricks from the vendor take a look at Veeco's homepage [1]

A rough overview of the performance of Dektak 8 stylus profiler

Purpose Profiler for measuring micro structures.
  • Single point profiles
  • Wafer mapping
  • Stress measurements by measuring wafer bow
  • Surface roughness on a line scan
Performance Scan range xy

Line scan x: 50 µm to 100 mm

Scan range z

50 Å to 1 mm

Resolution xy

down to 0.067 µm

Resolution z

1Å, 10Å, 40Å or 160Å (for ranges 65kÅ, 655 kÅ, 2620 kÅ and 1mm respectively)

Max. scan depth as a function of trench width W

1.2(W[µm]-5µm)

Hardware settings Tip radius
  • 5 µm 45o cone
Substrates Substrate size
  • up to 8"
Substrate material allowed
  • In principle all materials

Tencor stylus profiler

 
Tencor: positioned in cleanroom 4 - glass cage no. 3

Tencor P1 stylus profiler is a product of KLA-Tencor Corporation. It is usable for profiling surfaces of samples with structures in the micrometer range. It can measure in a specific point found with help from a high magnification video camera. It can also be used for stress measurements of thin films by measuring the wafer bow.

It is a very old system and should be treated with care.

Overview of the performance of Tencor P1 stylus profiler

Purpose Profiler for measuring micro structures.
  • Single point profiles
  • Stress measurements by measuring wafer bow
  • Surface roughness on a line scan
Performance Scan range xy

Line scan x: Full substrate size

Scan range z

<100 Å to ~0.3 mm

Resolution xy

up to 5900 data points per profile

Resolution z

1Å or 25Å

Max. scan depth as a function of trench width W

0.87(W[µm]-5µm)

Hardware settings Tip radius
  • 5 µm 60o cone
Substrates Substrate size
  • up to 4"
Substrate material allowed
  • In principle all materials

Comparing the profilers

Take a look at the topographic measurement page.