AFM picture of Cr layerdeposited with e-beam evaporation in Wordentec. Deposition rate 10 Å/s.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 08:37, 13 August 2008 | 795 × 628 (114 KB) | Kn (talk | contribs) | AFM picture of Cr layerdeposited with e-beam evaporation in Wordentec. Deposition rate 10 Å/s. |