Jump to content

File:Cr 150W 001mbar.JPG

From LabAdviser
Revision as of 11:33, 12 August 2008 by Kn (talk | contribs) (AFM picture of sputtered Cr layer 150 W and 0.001 mbar used)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Cr_150W_001mbar.JPG (file size: 393 KB, MIME type: application/msword)

Warning: This file type may contain malicious code. By executing it, your system may be compromised.

AFM picture of sputtered Cr layer 150 W and 0.001 mbar used

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeDimensionsUserComment
current11:33, 12 August 2008 (393 KB)Kn (talk | contribs)AFM picture of sputtered Cr layer 150 W and 0.001 mbar used

There are no pages that use this file.