Comparison of processes before and after the change of showerhead in December 2014
Process Before After
Wafer ID Comment SEM images Wafer ID Comment SEM images
rebe g4-14 black silicon recipe S004592 Wafer centre S004679 Wafer centre
S004592 Wafer edge S004679 Wafer edge