Revision as of 11:29, 29 September 2014 by Paphol (talk | contribs) (The percent of film non-uniformity variation with growth time in different temperature. (left) Over the boat and (right) over the wafer)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (938 × 384 pixels, file size: 62 KB, MIME type: image/png)

The percent of film non-uniformity variation with growth time in different temperature. (left) Over the boat and (right) over the wafer