Thickness measurer

 
Digital Thickness Measurer. Positioned in cleanroom 4

The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.

Doing a KOH etch can it be helpful to insure no over etching by making a thickness measurement doing the etch.

The user manual, technical information and contact information can be found in LabManager:

Thickness measurer

Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result have to be within ± 0.005 mm. The QC is preformed ones a year.

Equipment performance and process related parameters

Purpose

Thickness measurer

  • Wafer
  • Depths of larger grooves
  • Heigth of larger mesas

Performance

Thickness resolution

  • >5 µm

Process parameter range

Process Temperature

  • Room temperature
Process pressure
  • 1 atm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restriction.