Revision as of 10:03, 4 November 2013 by Khara (talk | contribs) (SU-8 etched with SU8aniso, anisotropy 0.8, etch rate ~400nm/min, antimony surface layer concentration <2%)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 943 pixels, file size: 116 KB, MIME type: image/jpeg)

SU-8 etched with SU8aniso, anisotropy 0.8, etch rate ~400nm/min, antimony surface layer concentration <2%