Specific Process Knowledge/Thermal Process/Jipelec RTP
Appearance
Jipelec - Rapid Thermal Processing
Feedback to this page: click here
The Jipelec is a rapid thermal processing oven. It should be used for fast and well-controlled annealing or alloying of samples. It is possible to use a pyrometer to control the temperature (of the carrier).
The user manual(s), technical information and contact information can be found in LabManager:
| Purpose | RTP annealing | |
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gasses on the system |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
A silicon carrier wafer with 1 µm oxide is always need (except for III-V materials)
|