- 15:47, 15 March 2011 Jml talk contribs uploaded File:WF 2B4 feb06 2011-060.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.3 recipe, Run ID 430 and 432, time 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 20 degs.)
- 15:47, 15 March 2011 Jml talk contribs uploaded File:WF 2B4 feb06 2011-030.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.3 recipe, Run ID 430 and 432, time 180 secs, BCl3 5, HBr 15, 2mtorr, 900/75 coil/platen, 20 degs.)
- 15:46, 15 March 2011 Jml talk contribs uploaded File:WF 2B3 feb06 2011-150.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.2 recipe, Run ID 426 and 428, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/60 coil/platen, 20 degs.)
- 15:46, 15 March 2011 Jml talk contribs uploaded File:WF 2B3 feb06 2011-120.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.2 recipe, Run ID 426 and 428, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/60 coil/platen, 20 degs.)
- 15:45, 15 March 2011 Jml talk contribs uploaded File:WF 2B3 feb06 2011-090.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.2 recipe, Run ID 426 and 428, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/60 coil/platen, 20 degs.)
- 15:45, 15 March 2011 Jml talk contribs uploaded File:WF 2B3 feb06 2011-060.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.2 recipe, Run ID 426 and 428, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/60 coil/platen, 20 degs.)
- 15:45, 15 March 2011 Jml talk contribs uploaded File:WF 2B3 feb06 2011-030.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.2 recipe, Run ID 426 and 428, time 120 secs, BCl3 5, HBr 15, 2mtorr, 900/60 coil/platen, 20 degs.)
- 15:43, 15 March 2011 Jml talk contribs uploaded File:WF 2B2 feb06 2011-150.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.1 recipe, Run ID 424 and 425 and 427, time 180 secs, BCl3 3, HBr 17, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:43, 15 March 2011 Jml talk contribs uploaded File:WF 2B2 feb06 2011-120.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.1 recipe, Run ID 424 and 425 and 427, time 180 secs, BCl3 3, HBr 17, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:43, 15 March 2011 Jml talk contribs uploaded File:WF 2B2 feb06 2011-090.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.1 recipe, Run ID 424 and 425 and 427, time 180 secs, BCl3 3, HBr 17, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:43, 15 March 2011 Jml talk contribs uploaded File:WF 2B2 feb06 2011-060.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.1 recipe, Run ID 424 and 425 and 427, time 180 secs, BCl3 3, HBr 17, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:43, 15 March 2011 Jml talk contribs uploaded File:WF 2B2 feb06 2011-030.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.1 recipe, Run ID 424 and 425 and 427, time 180 secs, BCl3 3, HBr 17, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:42, 15 March 2011 Jml talk contribs uploaded File:WF 2A4 feb06 2011-150.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.0 recipe, Run ID 417 and 418 and 419, time 150 secs, BCl3 5, HBr 15, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:42, 15 March 2011 Jml talk contribs uploaded File:WF 2A4 feb06 2011-120.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.0 recipe, Run ID 417 and 418 and 419, time 150 secs, BCl3 5, HBr 15, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:41, 15 March 2011 Jml talk contribs uploaded File:WF 2A4 feb06 2011-090.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.0 recipe, Run ID 417 and 418 and 419, time 150 secs, BCl3 5, HBr 15, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:41, 15 March 2011 Jml talk contribs uploaded File:WF 2A4 feb06 2011-060.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.0 recipe, Run ID 417 and 418 and 419, time 150 secs, BCl3 5, HBr 15, 2mtorr, 900/50 coil/platen, 20 degs.)
- 15:41, 15 March 2011 Jml talk contribs uploaded File:WF 2A4 feb06 2011-030.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano3.0 recipe, Run ID 417 and 418 and 419, time 150 secs, BCl3 5, HBr 15, 2mtorr, 900/50 coil/platen, 20 degs.)
- 11:43, 15 March 2011 Ast talk contribs changed group membership for Bilal from (none) to nanotech
- 15:00, 10 March 2011 Ast talk contribs changed group membership for Pfos from (none) to nanotech
- 16:21, 8 March 2011 Ast talk contribs changed group membership for Alijo from (none) to nanotech
- 10:15, 8 March 2011 Ast talk contribs changed group membership for Hsch from (none) to fotonik
- 14:51, 7 March 2011 Choi talk contribs uploaded File:Imm.jpg (Picture of the IMM.)
- 14:39, 7 March 2011 Jml talk contribs uploaded File:WF 2A-5 feb06 2011-150.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano4.0 recipe, Run ID 435 and 436, time 90 secs, Cl2 20, 2mtorr, 900/60 coil/platen, 20 degs.)
- 14:39, 7 March 2011 Jml talk contribs uploaded File:WF 2A-5 feb06 2011-120.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano4.0 recipe, Run ID 435 and 436, time 90 secs, Cl2 20, 2mtorr, 900/60 coil/platen, 20 degs.)
- 14:39, 7 March 2011 Jml talk contribs uploaded File:WF 2A-5 feb06 2011-090.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano4.0 recipe, Run ID 435 and 436, time 90 secs, Cl2 20, 2mtorr, 900/60 coil/platen, 20 degs.)
- 14:38, 7 March 2011 Jml talk contribs uploaded File:WF 2A-5 feb06 2011-060.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano4.0 recipe, Run ID 435 and 436, time 90 secs, Cl2 20, 2mtorr, 900/60 coil/platen, 20 degs.)
- 14:38, 7 March 2011 Jml talk contribs uploaded File:WF 2A-5 feb06 2011-030.jpg (Etching of nanostructures in Si using the ICP metal etcher: Sinano4.0 recipe, Run ID 435 and 436, time 90 secs, Cl2 20, 2mtorr, 900/60 coil/platen, 20 degs.)
- 11:21, 25 February 2011 Ast talk contribs changed group membership for Wan from (none) to nanotech
- 11:16, 25 February 2011 Jml talk contribs uploaded File:Crystalbond2.jpg (Problems with crystalbond on Pegasus: A wafer bonded to a carrier has slided off during process.)
- 13:02, 24 February 2011 Ast talk contribs changed group membership for Zhe from (none) to nanotech
- 12:33, 24 February 2011 Ast talk contribs changed group membership for Remn from (none) to nanotech
- 11:05, 24 February 2011 Ast talk contribs changed group membership for Makei from (none) to danchip
- 16:16, 23 February 2011 Jml talk contribs uploaded File:WF 2F-6 dec092010-30 nm.jpg (ICP metal etcher: Starting point for development of Si nano etch recipe.)
- 16:16, 23 February 2011 Jml talk contribs uploaded File:WF 2F-6 dec092010-120 nm.jpg (ICP metal etcher: Starting point for development of Si nano etch recipe.)
- 14:17, 23 February 2011 Ast talk contribs changed group membership for Joer from (none) to nanotech
- 11:51, 22 February 2011 Ast talk contribs changed group membership for Ales from (none) to nanotech
- 12:53, 21 February 2011 Ast talk contribs changed group membership for Cdp from (none) to nanotech
- 10:08, 16 February 2011 Ast talk contribs changed group membership for Imso from (none) to fotonik
- 15:10, 11 February 2011 Jehan talk contribs uploaded File:Process flow template.doc (Process flow template/ Procesfølge skabelon)
- 12:31, 10 February 2011 Ast talk contribs changed group membership for Ekm from (none) to nanotech
- 12:25, 10 February 2011 Ast talk contribs changed group membership for Suh from (none) to nanotech
- 11:47, 10 February 2011 Elk talk contribs uploaded File:5ml SU8 2002 in32ml cycl.PNG
- 11:42, 10 February 2011 Elk talk contribs uploaded File:5ml SU8 2002 in 32ml cycl.PNG (Spinning curve for diluted SU8 2002.)
- 11:54, 9 February 2011 Ast talk contribs changed group membership for Giogi from (none) to fotonik
- 11:32, 9 February 2011 Ast talk contribs changed group membership for Greal from (none) to industry
- 11:24, 9 February 2011 Ast talk contribs changed group membership for Mahuf from (none) to industry
- 12:19, 8 February 2011 Ast talk contribs changed group membership for Zolba from (none) to industry
- 11:23, 8 February 2011 Ast talk contribs changed group membership for Paom from (none) to nanotech
- 11:02, 8 February 2011 Ast talk contribs changed group membership for Afp from (none) to nanotech
- 15:50, 1 February 2011 Ast talk contribs changed group membership for Gllk from (none) to nanotech