- 09:59, 10 December 2012 Khr talk contribs uploaded File:IBE-Si-CA-contour.jpg (The angle in the corner of an etch structure showed a dependency on Beam and Acc. Voltage and Incident angle, with no interactions between any parameters. Values found on the plot should always be tested before use.)
- 09:57, 10 December 2012 Khr talk contribs uploaded File:IBE-Si-ER-contour.jpg (IBE etch rate only shows a dependency on Beam Current and Beam Voltage. Values found on the plot should always be tested before use.)
- 17:18, 15 November 2012 Khr talk contribs uploaded File:IBE magnetic DoE Corner Angle.jpg (Design of Experiment calculated corner angle of etch magnetic stack)
- 17:17, 15 November 2012 Khr talk contribs uploaded File:IBE magnetic DoE etch rate.jpg (Design of Experiment calculated etch rate contour plot.)
- 12:03, 12 November 2012 Khr talk contribs uploaded File:Silicon-IBE-bad-b21.jpg (SEM picture of IBE with bad corner definition (b21-19))
- 12:02, 12 November 2012 Khr talk contribs uploaded File:Silicon-IBE-good-b17.jpg (SEM picture of silicon IBE with good corner definition (b17-14))
- 12:00, 12 November 2012 Khr talk contribs uploaded File:Silicon-IBE-good-b17.tif
- 08:30, 9 October 2012 Khr talk contribs uploaded File:KHARA-MLS-DoE.png
- 15:14, 27 September 2012 Khr talk contribs uploaded File:SIMS end point detection.png (IBE etch of magnetic stack. Experiments done by Kristian Hagsted Rasmussen email: kristian.rasmussen@nanotech.dtu.dk )
- 15:01, 27 September 2012 Khr talk contribs uploaded File:IBE magnetic stack A3-13.jpg (IBE etch of magnetic stack. Experiments done by Kristian Hagsted Rasmussen email: kristian.rasmussen@nanotech.dtu.dk )
- 15:01, 27 September 2012 Khr talk contribs uploaded File:IBE magnetic stack A16-13.jpg (IBE etch of magnetic stack. Experiments done by Kristian Hagsted Rasmussen email: kristian.rasmussen@nanotech.dtu.dk )
- 14:57, 27 September 2012 Khr talk contribs uploaded File:IBE magnetic stack A19-13.jpg (IBE etch of magnetic stack. Experiments done by Kristian Hagsted Rasmussen email: kristian.rasmussen@nanotech.dtu.dk)