The profiles of the 211 nm thick zep resist wafers (The E-batch of march 23 2011). The wafers have been over-exposed in the E-beam (400 µC/cm2) to make sure that all structures are opened - therefore the 30, 60, 90, 120 and 150 nm lines are somewhat wider.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current15:18, 7 April 2011Thumbnail for version as of 15:18, 7 April 20111,024 × 768 (122 KB)Jml (talk | contribs)The profiles of the 211 nm thick zep resist wafers (The E-batch of march 23 2011). The wafers have been over-exposed in the E-beam (400 µC/cm2) to make sure that all structures are opened - therefore the 30, 60, 90, 120 and 150 nm lines are somewhat wide