File:UnCoatedBlockCopolymer-2e.jpg
Appearance
Size of this preview: 651 × 600 pixels. Other resolution: 1,024 × 943 pixels.
Original file (1,024 × 943 pixels, file size: 224 KB, MIME type: image/jpeg)
SEM FEI LoVac image of a block copolymer: Fifth single scan of specific area.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 12:51, 5 February 2009 | 1,024 × 943 (224 KB) | Jml (talk | contribs) | SEM FEI LoVac image of a block copolymer: Fifth single scan of specific area. |