File:Rs AmorBor vs PolyBor .png
Appearance
Size of this preview: 739 × 600 pixels. Other resolution: 1,172 × 951 pixels.
Original file (1,172 × 951 pixels, file size: 28 KB, MIME type: image/png)
Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour and Boron doped a-Si using "AMORBOR" recipe, Deposition time : 75 minutes, B2H6 flow at 7sccm, anneal: 950C 1hour. (Result from Trine H. Christensen DTU Space)
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 10:30, 19 February 2015 | 1,172 × 951 (28 KB) | Paphol (talk | contribs) | Sheet resistance on Boron doped poly-si using "POLYBOR" recipe, deposition time : 30 minutes, B2H6 flow at 7 sccm and 30 sccm, anneal : 950C 1 hour and Boron doped a-Si using "AMORBOR" recipe, Deposition time : 75 minutes, B2H6 flow at 7sccm, anneal: 9... |
You cannot overwrite this file.
File usage
There are no pages that use this file.