Gatan OneView camera and GMS3


Here are a few information on the OneView camera and the control in GMS3:


Headline text

General info: - CMOS camera with 4096 x 4096px (pixel size: 15µm) --> 61.4 x 61.4mm sensor size - Imaging mode: 25fps for full 4k x 4k resolution (single frame exposure time: 0.04s); 100fps @ 2k x 2k; 200fps @ 1k x 1k; 300fps @ 512 x 512 - Diffraction mode:



Go to "Customs" and "SetDoseCalibrationTag_OneView_mod-DTU"

Run script


2. Type in the high tension the microscope is running in the pop-up window

Select high tension


3. Don't change the conversion factor; just click on "OK"

Don't change conversion factor