Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/SIMS settings
Appearance
Feedback to this page: click here
Made by bge@danchip in 2015
| SIMS setting for different materials | ||
| Lower plate | Upper plate | |
|---|---|---|
| Ti | -1 | |
| Si | -1 | (2) |
| Al | -1 | 1 |
| Cr | -1 | |
| Ni | -6 | |
Feedback to this page: click here
Made by bge@danchip in 2015
| SIMS setting for different materials | ||
| Lower plate | Upper plate | |
|---|---|---|
| Ti | -1 | |
| Si | -1 | (2) |
| Al | -1 | 1 |
| Cr | -1 | |
| Ni | -6 | |