Jump to content

File:NiV-Roughness-Power.png

From LabAdviser
Revision as of 16:10, 3 January 2017 by Paphol (talk | contribs) (Paphol uploaded a new version of "File:NiV-Roughness-Power.png": NiV roughness VS Power)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

NiV-Roughness-Power.png (632 × 458 pixels, file size: 13 KB, MIME type: image/png)

NiV film Roughness VS sputtering power

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current16:10, 3 January 2017Thumbnail for version as of 16:10, 3 January 2017632 × 458 (13 KB)Paphol (talk | contribs)NiV roughness VS Power
09:55, 3 January 2017Thumbnail for version as of 09:55, 3 January 2017632 × 458 (14 KB)Paphol (talk | contribs)NiV film Roughness VS sputtering power