Jump to content

File:Process parameters for AlN.png

From LabAdviser
Revision as of 10:37, 8 October 2015 by Paphol (talk | contribs) (Parameters used in Cryofox PVD co-sputter/evaporation)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,281 × 259 pixels, file size: 34 KB, MIME type: image/png)

Parameters used in Cryofox PVD co-sputter/evaporation

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current10:37, 8 October 2015Thumbnail for version as of 10:37, 8 October 20151,281 × 259 (34 KB)Paphol (talk | contribs)Parameters used in Cryofox PVD co-sputter/evaporation

There are no pages that use this file.

Metadata