Revision as of 10:04, 4 November 2013 by Khara (talk | contribs) (SU-8 etched with SU8iso, anisotropy 0.3, etch rate ~170nm/min, antimony surface layer concentration <2.75%)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Original file (1,024 × 943 pixels, file size: 133 KB, MIME type: image/jpeg)

SU-8 etched with SU8iso, anisotropy 0.3, etch rate ~170nm/min, antimony surface layer concentration <2.75%

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current10:04, 4 November 2013Thumbnail for version as of 10:04, 4 November 20131,024 × 943 (133 KB)Khara (talk | contribs)SU-8 etched with SU8iso, anisotropy 0.3, etch rate ~170nm/min, antimony surface layer concentration <2.75%