Specific Process Knowledge/Etch/Etching of Aluminium
Appearance
Etching of Aluminium
Etching of aluminium is done wet at Danchip. We have two different solutions:
- HO:HPO 1:2 at 50 oC
- Pre-mixed etch solution: PES 77-19-04 at 20 oC
| Aluminium Etch 1 | Aluminium Etch 2 | |
|---|---|---|
| General description |
|
|
| Chemical solution | ||
| Possible masking materials: |
|
|
| Etch rate |
~100 nm/min (Pure Al) |
~60(??) nm/min |
| Batch size |
|
|
| Size of substrate |
|
|
| Allowed materials |
|
|