- 11:28, 30 January 2023 Jehem talk contribs created page Specific Process Knowledge/Lithography/Coaters/Spin Coater: Gamma DUV processing (Created page with "=General Process Information= Processing using Spin Coater: Süss stepper is divided into two parts: *Spin coating *Soft baking ==Spin coating== The process of spin coating on Spin Coater: GSüss stepper consists of a selection of the following steps: *Acceleration to a low spin speed if dynamic dispense is used *Resist dispense *Spin-off The wafer is first centered on the spindle chuck and held in place by vacuum. If static dispense is specified in the process, the sp...")