- 19:28, 14 December 2022 Eves talk contribs created page Specific Process Knowledge/Thin film deposition/Deposition of Tungsten/Sputtering of W in Sputter Coater 3 (Created page with "Sputter Coater 3 is mainly used for sample preparation before SEM inspection. Usually, Au is sputtered on dielectric surfaces to compensate for charge build-up. Alternatively, many other materials can be sputtered if the setup allows (you need to have a turbo pump and Ar gas). Gold can be deposited even in pure oxygen plasma and only with roughing pumps. Fortunately, Sputter Coater 3 located in the basement of building 346, has both a turbo pump and an Ar working gas sou...")