Combined display of all available logs of LabAdviser. You can narrow down the view by selecting a log type, the username (case-sensitive), or the affected page (also case-sensitive).
- 15:15, 18 June 2020 Bghe talk contribs deleted page Specific Process Knowledge/Thin film deposition/ALD Picosun R200/AlN deposition using ALD2/Acceptance test AlN (content was: "==AlN with N<sub>2</sub> plasma== <!-- Experiment 161102A --> The test was done with 300 cycles at 350 °C where the growth rate was measured to be '''0.0625 nm/cycl..." (and the only contributor was "Eves"))