==Distribution Chamber (Genmark robot)== | ==Distribution Chamber (Genmark robot)== | ||
The load-lock and process chambers PC1 and PC3 are all connected through the common distribution chamber. The robot arm can transfer the sample to the selected destination. During normal operation, the chamber is pumped to a base pressure ensuring the safe transfer of the sample between chambers and load-lock without breaking a vacuum. | The load-lock and process chambers PC1 and PC3 are all connected through the common distribution chamber. The robot arm can transfer the sample to the selected destination. During normal operation, the chamber is pumped to a base pressure ensuring the safe transfer of the sample between chambers and load-lock without breaking a vacuum. The unit is conectedto its own turbo-pump. | ||