Cluster-based multi-chamber high vacuum sputtering deposition system is a robotic cluster tool with two deposition chambers sharing the same distribution trasfer station and the load-lock. The equipment has been installed and accepted in clean-room during January 2020. The purpose of the tool is to deposite variety of materials using DC/RF/PulseDC/HIPIMS magnetron sputtering with or without RF substrate bias. In modul A or process chamber 1 (PC1) it is possible to deposit any materials using 6 x 3” magnetrons sourses with N2 or O2 reactive gases. Modul B or process chamber 2 is dedicated to ony oxygen free materials - nitrides and metals it is eqipted with 1 x 4” + 2 x 3” magnetrons and supplied with N2 process gas for reactive deposition. Both chambers allow heating of substrates up to 600 C. | Cluster-based multi-chamber high vacuum sputtering deposition system is a robotic cluster tool with two deposition chambers sharing the same distribution trasfer station and the load-lock. The equipment has been installed and accepted in clean-room during January 2020. The purpose of the tool is to deposite variety of materials using DC/RF/PulseDC/HIPIMS magnetron sputtering with or without RF substrate bias. In modul A or process chamber 1 (PC1) it is possible to deposit any materials using 6 x 3” magnetrons sourses with N2 or O2 reactive gases. Modul B or process chamber 2 is dedicated to ony oxygen free materials - nitrides and metals it is eqipted with 1 x 4” + 2 x 3” magnetrons and supplied with N2 process gas for reactive deposition. Both chambers allow heating of substrates up to 600 <sup>o</sup>C. | ||
[[image:Kaempe_Lesker_image_front_page1.jpg|450x450px|right|thumb|Cluster-based multi-chamber high vacuum sputtering deposition system. View from service room Ax-1.]] | [[image:Kaempe_Lesker_image_front_page1.jpg|450x450px|right|thumb|Cluster-based multi-chamber high vacuum sputtering deposition system. View from service room Ax-1.]] | ||
Manufacture: Kurt J. Lesker | <b> Manufacture:</b> Kurt J. Lesker Company | ||
Model: 2017 PRO Line PVD75 thin film deposition cluster system | <b> Model:</b> 2017 PRO Line PVD75 thin film deposition cluster system | ||