LabAdviser/Technology Research/Fabrication of Hyperbolic Metamaterials using Atomic Layer Deposition: Difference between revisions
Appearance
| Line 113: | Line 113: | ||
===Conductive oxides trench structures as hyperbolic metamaterials in mid-infrared range=== | ===Conductive oxides trench structures as hyperbolic metamaterials in mid-infrared range=== | ||
O. Takayama, <u>E. Shkondin</u>, M. E. A. Panah, T. Reän, R. Malureanu, F. Jensen, A. V. Lavrinenko <br> | O. Takayama, <u>E. Shkondin</u>, M. E. A. Panah, T. Reän, R. Malureanu, F. Jensen, A. V. Lavrinenko <br> | ||
Abstract from 14th International Conference of Near-Field Optics, Nanophotonics and Related Techniques, Hamamatsu, Japan | 2016. Abstract from 14th International Conference of Near-Field Optics, Nanophotonics and Related Techniques, Hamamatsu, Japan | ||
===Fabrication of hollow coaxial ZnAl2O4 high aspect ratio freestanding nanopillars based on the Kirkendall effect=== | ===Fabrication of hollow coaxial ZnAl2O4 high aspect ratio freestanding nanopillars based on the Kirkendall effect=== | ||
| Line 124: | Line 124: | ||
===TiO2 and Al2O3 ALD grown multilayers for subwavelength photonics=== | ===TiO2 and Al2O3 ALD grown multilayers for subwavelength photonics=== | ||
<u>E. Shkondin</u>, F. Jensen, A. V. Lavrinenko, M. D. Mar, P. V. Larsen, R. Malureanu, S. Zhukovsky, A. Andryieuski, O. Takayama <br | <u>E. Shkondin</u>, F. Jensen, A. V. Lavrinenko, M. D. Mar, P. V. Larsen, R. Malureanu, S. Zhukovsky, A. Andryieuski, O. Takayama <br> | ||
DTU's Sustain Conference 2015, Technical University of Denmark, Kgs. Lyngby, Denmark (2015) | 2015. DTU's Sustain Conference 2015, Technical University of Denmark, Kgs. Lyngby, Denmark (2015) | ||
===Deep subwavelength photonic multilayers fabricated by atomic layer deposition=== | ===Deep subwavelength photonic multilayers fabricated by atomic layer deposition=== | ||
| Line 137: | Line 137: | ||
===Depositing Materials on the Micro- and Nanoscale=== | ===Depositing Materials on the Micro- and Nanoscale=== | ||
M. D. Mar, B. Herstrøm, <u>E. Shkondin</u>, P. Pholprasit, F. Jensen <br> | M. D. Mar, B. Herstrøm, <u>E. Shkondin</u>, P. Pholprasit, F. Jensen <br> | ||
DTU's Sustain Conference 2014, Technical University of Denmark, Kgs. Lyngby, Denmark (2014) | 2014. DTU's Sustain Conference 2014, Technical University of Denmark, Kgs. Lyngby, Denmark (2014) | ||