Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride/Deposition of Silicon Nitride using PECVD: Difference between revisions

Bghe (talk | contribs)
Bghe (talk | contribs)
Line 133: Line 133:
|-
|-
|Refractive Index
|Refractive Index
|1.909 - 2.028
|2.02 - 2.04
|}
|}
|-
|-