|1SiN | |1SiN | ||
| | | | ||
Deposition rate in the middle of two wafers: '''49nm/min+-1nm/min''' | Deposition rate in the middle of two wafers: '''49nm/min+-1nm/min''' (2015-04-24 BGHE) <br> | ||
In the middel: '''72.6-76.4 nm/min''' (2014-08-13 BGHE) <br> | In the middel: '''72.6-76.4 nm/min''' (2014-08-13 BGHE) <br> | ||
Variation over 3 wafers: '''71.4-78.6 nm/min''' (2014-08-13 BGHE) | Variation over 3 wafers: '''71.4-78.6 nm/min''' (2014-08-13 BGHE) | ||