Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride/Deposition of Silicon Nitride using PECVD: Difference between revisions
Appearance
| Line 57: | Line 57: | ||
| | | | ||
| | | | ||
| | |||
| | |||
| | |||
|- | |||
|1SiN | |||
| | |||
In the middel: '''72.6-76.4 nm/min''' (2014-08-13 BGHE) <br> | |||
Variation over 3 wafers: '''71.4-78.6 nm/min''' (2014-08-13 BGHE) | |||
| | |||
| | |||
'''~5%''' in the middel (4") (2014-08-13 BGHE)<br> | |||
'''~10%''' over 3 wafers (2014-08-13 BGHE) | |||
| | | | ||
| | | | ||